Item |
GRLC 75 |
GRLC 80 |
GRLC 85 |
GRLC 95 |
Service TempºC |
1650 |
1700 |
1750 |
1780 |
Bulk Density (g/cm3) (Dried at 110ºC) |
2.55 |
2.6 |
2.7 |
3.0 |
CCS 110ºC (Mpa) 1100ºC 1500ºC |
65 75 80 |
70 80 85 |
80 90 100 |
90 95 110 |
MOR 110ºC (Mpa) 1100ºC 1500ºC |
9 10 11 |
10 11 12 |
11 12 13 |
13 14 15 |
Max Grain Size (mm) |
6 |
6 |
6 |
6 |
Chemical Analysis(%) Al2O3 Cao Fe2O3 |
75 2-3 2.4 |
80 2-3 2.0 |
85 2-3 1.8 |
95 2-3 1.5 |
Application Guidelines Mixer Placement Water/Mixer Temp ºC Mixing Time(Min): Dry/Wet |
P V 20±5 2/5 |
P V 20±5 2/5 |
P V 20±5 2/5 |
P V 20±5 2/5 |
Water % (Typical) |
7-9 |
7-9 |
6-8 |
6-7 |
Low cement castable is based on the use of low calcium aluminate cement content, and they are used in many applications that require high refractoriness, corrosion resistance and abrasion resistance. They possess a uniform structure with low porosity; have high temperature strength throughout the low and intermediate temperature range.
The content of CaO of low cement castable is usually less than 3%,so it insure the castable have a good strength in mid-temperature.